SIAGIAN, SONY HADI ISMANTO (2013) KAJIAN INDEKS KECEPATAN PENGEBORAN TERHADAP PENGARUH SIFAT MEKANIK BATUGAMPING DI DAERAH ISTIMEWA YOGYAKARTA. Other thesis, UPN "Veteran" Yogyakarta.
Preview |
Text
Ringkasan Sony H. I. Siagian -112090039.pdf Download (22kB) | Preview |
Abstract
Pengeboran dalam kegiatan penambangan digunakan antara lain untuk
pembuatan lubang ledak serta untuk menggunakan lubang bor tersebut untuk
tujuan lain selain peledakan. Dalam kegiatan peledakan, cepat lambatnya
penyediaan lubang ledak akan berpengaruh terhadap kelancaran kegiatan
peledakan. Sementara itu, cepat lambatnya penyediaan lubang ledak dipengaruhi
oleh kecepatan alat bor untuk menembus batuan. Kecepatan pengeboran
dipengaruhi oleh sifat mekanik batugamping, dimana batugamping pada Formasi
Sentolo di Dusun Diran, Desa Sidorejo, Kecamatan Lendah, Kabupaten
Kulonprogo berbeda dengan batugamping pada Formasi Oyo di Dusun Krunggo,
Desa Banyusoco, Kecamatan Playen, serta Formasi Wonosari di Dusun Jambu,
Desa Hargosari, Kecamatan Tanjungsari Kabupaten Gunung Kidul, Provinsi
Yogyakarta. Sehingga perlu dilakukan penelitian di laboratorium untuk
mengetahui korelasi data pengujian dengan Drilling Rate Index sebagai parameter
drillabilitas batuan.
Pengujian di laboratorium yang dilakukan antara lain sifat fisik, sifat
mekanik, sifat dinamik, serta brittleness test dan drill test. Data yang diperoleh
dikorelasikan dan dikaji untuk mengetahui pengaruh sifat mekanik terhadap
kecepatan pengeboran batugamping dengan parameter Drilling Rate Index.
Berdasarkan hasil pengujian diketahui bahwa Batugamping Formasi Oyo
dengan nilai DRI 29,69 (Low), 30,44 (Low), 31,04 (Low), Formasi Wonosari
dengan nilai DRI 32,19 (Low), 34,94 (Low), 36,67 (Low), serta Formasi Sentolo
dengan nilai DRI 69,41 (Very High), 69,58 (Very High), 70,51 (Very High). Dari
nilai DRI dapat ditarik kesimpulan bahwa Formasi Oyo paling sulit untuk
ditembus oleh mata bor dibandingkan dengan Formasi Wonosari dan Formasi
Sentolo. Dari hasil penelitian ini juga didapatkan persamaan yang dapat
digunakan untuk mengetahui nilai DRI dari nilai kuat tekan uniaksial yaitu
DRI = 157,2 σc
-0,44 , kemudian dari nilai kuat tarik yaitu DRI = 332 σt
-1,71 serta
dari nilai Brittleness Index yaitu DRI = 102,6 BI-0,50.
Drilling in mining operations is used to make an explosive hole and also
for the other purpose. In the blasting activity, the increase of speed of drill will
affect the operation of the blasting. Otherwise, the increasing of speed to make the
hole is affected by the speed of drills to penetrate the rock. The speed of drilling is
affected by the mechanic properties of limestone, which the Sentolo formation of
limestone in Diran Region, Sidorejo Village, Lendah District, Kulonprogo
Regency is different with the Oyo formation in Krunggo Region, Banyusoko
Village, Playen District, and also the Wonosari formation in Jambu Region,
Hargosari Village, Tanjungsari District, Gunung Kidul Kulonprogo Regency ,
Daerah Istimewa Yogyakarta Province. So it is necessary to do research in the
laboratory to determine the correlation of the test data by drilling rate index as a
parameter of the rock drillability.
The various tests conducted in the laboratory include the physical
properties test, mechanical properties test, dynamic properties test, brittleness test
and drill test. The obtained data correlated and analyzed to determine the effect of
the mechanical properties to the limestones the drilling speed with Drilling Rate
Index parameter.
Based on the test, the result shows that the Oyo Limestone Formation has
29,69 (Low), 30,44 (Low), 31,04 (Low) DRI values, the Wonosari Limestone
Formation has 32,19 (Low), 34,94 (Low), 36,67 (Low) DRI values, and the
Sentolo Limestone Formation has 69,41 (Very High), 69,58 (Very High), 70,51
(Very High) DRI values. From the DRI values, it can be deduced that Oyo
Formation is the most difficult to penetrated by the drill bit comparison with the
Wonosari Formation and Sentolo Formation. From the results of this study, we
also found a formulation that can be used to determine DRI values from uniaxial
compressive strength, the formula is DRI = 157,2 σc
-044, then the DRI values from
the tensile strength is DRI = 332 σt
-1,71, and also the DRI values from the value of
Brittleness Index is DRI = 102,6 BI-0,50.
Item Type: | Thesis (Other) |
---|---|
Subjek: | T Technology > TN Mining engineering. Metallurgy |
Divisions: | x. Faculty of Engineering, Science and Mathematics > School of Engineering Sciences |
Depositing User: | Eko Suprapti |
Date Deposited: | 23 May 2016 07:47 |
Last Modified: | 23 May 2016 07:47 |
URI: | http://eprints.upnyk.ac.id/id/eprint/2162 |
Actions (login required)
![]() |
View Item |